Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_03f1df91fd821534ee794e3679e57fea |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D2323-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2201-052 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D2325-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2201-0546 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2323-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D2323-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2201-0543 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D71-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D67-0009 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-28 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D67-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D71-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-28 |
filingDate |
1986-02-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ea52e8f6d0496933948edfc8957dfa98 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_22625486b4c932b9032c862ee1047cd3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f7d1ddf8f55f8449c7fbf5d77deab337 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0fdcc1fb28adeabd99715895f61054e7 |
publicationDate |
1986-09-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-0193318-A2 |
titleOfInvention |
Microporous membrane of ultra-high molecular weight alpha-olefin polymer |
abstract |
A micro-porous membrane of ultra-high-molecular-weight alpha-olefin polymer having a weight-average molecular weight greater than 5 x 10<sup>5</sup>, the micro-porous membrane having through holes 0.01 to 1 micrometer in average pore size, with a void ratio from 30 to 90% and being orientated such that the linear draw ratio in one axis is greater than two and the areal draw ratio is greater than ten. The micro-porous membrane is obtained by forming a gel-like object from a solution of an alpha-olefin polymer having a weight-average molecular weight greater than 5 x 10<sup>6</sup>, removing at least 10 wt% of the solvent contained in the gel-like object so that the gel like object contains 10 to 90 wt% of alpha-olefin polymer, orientating the gel-like object at a temperature lower than that which is 10°C above the melting point of the alpha-olefin polymer, and removing the residual solvent from the orientated product. A film is produced from the orientated product by pressing the orientated product at a temperature lower than that of the melting point of the alpha-olefin polymer. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0765900-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0288874-A2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0288021-A2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0355214-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0288874-A3 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0289859-A2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4861644-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0288021-A3 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0289859-A3 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0528582-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4833172-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5830554-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5882518-A |
priorityDate |
1985-02-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |