Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_07b3f7652bef102674d95b2457346b0a |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D7-142 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D125-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-088 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D125-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D135-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-00 |
filingDate |
1985-12-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0f2679cbec95fef329f5cf1d21e9752b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_99ef5865fbbb254115f6f8997b619b25 |
publicationDate |
1986-07-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-0186113-A2 |
titleOfInvention |
Use of fugitive plasticizer in autodepositing composition |
abstract |
An autodeposition composition comprising water and resin solids, characterized in that the resin has a glass transition temperature of at least 55°C and in that a substantially water insoluble fugitive plasticizer is present in an amount sufficient to reduce the cracking tendency of autodeposited coatings formed from the composition. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-9106375-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-9213038-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5114751-A |
priorityDate |
1984-12-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |