abstract |
The invention relates to a process for the production of moldings based on a mixture of 80 to 95% by weight of at least one 1,2-polyepoxide and 5 to 20% by weight of a special polyester urethane, a usual amount of a 1,2-epoxy resin hardener as well as, where appropriate, conventional additives by curing at room temperature or elevated temperatures. The molded articles produced by the process of the invention have increased impact and shock resistance as well as improved flexibility and crack resistance. |