http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0155589-A2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5c24684033fba97d1ad845ce453a57e3 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D201-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D3-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-26 |
filingDate | 1985-03-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d467b427f45999b7f6941a783f6dd24f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9593ea72c4bf186346af942f98f0d7ea http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5353b4729dda5d0886732579ebe59f44 |
publicationDate | 1985-09-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-0155589-A2 |
titleOfInvention | Process for producing coatings on surfaces of solid materials by baking |
abstract | Process for the stoving coating of surfaces of solid materials by applying the required amount of an aqueous dispersion to the surface to be coated, the dispersion containing as binder a coarse, crosslinkable dispersion copolymer made from olefinically unsaturated monomers and optionally other conventional paint formulation components and the crosslinkable dispersion copolymer made from a mixture of at least 2 components, which may contain the same or different monomer units, of which at least one component A, which is coarse, has a relatively low average molecular weight and at least one component B, which can be coarse or fine, has a relatively high average molecular weight, and the weight ratio of components A: B is preferably in the range from 99: 1 to 1: 1. Drying the amount of dispersion applied at a temperature below its minimum film-forming temperature and crosslinking the dried coating by baking at a temperature above the glass transition temperature of the copolymer. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0238037-A2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0300612-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0236879-A2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0236879-A3 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0238037-A3 |
priorityDate | 1984-03-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 109.