abstract |
Thermoplastic, impact-resistant molding compositions made from (A) 5 to 80 parts by weight of a graft product from 70 to 30% by weight of a mixture of a vinylaromatic and acrylonitrile and / or methacrylonitrile to 30 to 70% by weight of a rubber with a glass transition temperature of below -10 ° C so graft and (B) 20-95 parts by weight of a terpolymer of styrene and / or a-methylstyrene, p-methylstyrene and acrylonitrile and / or methacrylonitrile, the terpolymer having been prepared by bulk polymerization, and a Process for their production. |