http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0083575-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a526baeaf0a6e90f4a91d4dbfd619756 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F36-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08C19-44 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F236-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F236-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F36-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08C19-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-04 |
filingDate | 1983-01-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_953c2a47a92fc6c275b1c7be11afd999 |
publicationDate | 1983-07-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-0083575-A1 |
titleOfInvention | Increasing the reactivity of coupling homopolymers |
abstract | There is disclosed a process for the preparation of elastomeric polymers which comprises contacting at least one conjugated diolefinic monomer selected from the group consisting of isoprene, piperylene, 2-ethyl-1,3-butadiene, 2,3-dimethyl--1,3-butadiene and 1,3-butadiene, mixed with at least one polyvinyl aromatic coupling compound selected from the group of o, m and p-divinylbenzene, 1,2,4-trivinylbenzene, 1,8-divinylnaphthalene, 1,2-divinyl-3,4-dimethylbenzene, 2,4-divinylbiphenyl, 3,5,4'-trivinylbiphenyl and 1,3,5-trivinylbenzene under solution polymerization conditions with an organolithium catalyst, in which the amount of polyvinyl aromatic coupling compound ranges from about 1.0 to about 6 vinyl groups per mole of active lithium catalyst used, in which the living polymer is treated with (A) a polar compound selected from the group consisting of ethylene glycol dimethyl ether (glyme), diethylene glycol dimethyl ether (diglyme), triethylene glycol dimethylether (triglyme), tetraethylene glycol dimethyl ether (tetraglyme), 2,3-dimethyoxybutane, N,N,N',N'-tetramethylethylene-diamine (TMEDA), tri-n-butylphosphine and hexamethylphosphoric triamide (HMPA), in which the molar ratio of the said polar compounds to the active lithium ranges from about 0.01/1 to about 20/1 or (B) a polar compound selected from the group consisting of tetrahydrofuran, diethyl ether, triethylamine, 1,4-diazabicyclo-2.2.2-octane (DABCO), p-dioxane, tri-n-butylamine and N,N'-dimethyl-piperazine, in which the molar ratio of the said polar compounds to the active lithium ranges from about 0.5/1 to about 100/1. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0211395-A1 |
priorityDate | 1982-01-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 141.