http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0015744-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_79b5f9d76648dfc226a261cfb970de9c |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2991 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-1134 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-1131 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-113 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-10 |
filingDate | 1980-03-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_98ab6fdc5cffee9737139da2f9009fd2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7cab907cddbbd81e1ac1f9babf1a9f13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a8df7c2ee32fba72e58f3dc234145be2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1d637566a68fbbd5a321d2102690dac2 |
publicationDate | 1980-09-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-0015744-A1 |
titleOfInvention | Process of preparing coated carrier particles for electrostatographic developers |
abstract | A process of preparing coated carrier particles for electrostatographic developer coated carrier particles for use in the development of electrostatic latent images are provided by mixing carrier core materials with powdered thermoplastic resin particles having a size of between 0.1 micron and 30 microns, and comprising between 0.05 and 3 percent by weight of the coated carrier particles. The carrier core materials are mixed with the resin particles until the resin particles mechanically and/or electrostatically adhere to the core materials and the mixture is heated to a temperature of between 160°C and 345 °C for between 120 minutes and 20 minutes so that the resin particles melt and fuse to the carrier core materials. The coated carrier particles are cooled, classified to the desired particle size, and mixed with finely-divided toner particles to form a developer mixture. The process is especially advantageous for coating carrier particles with resin materials having poor solubility characteristics. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0286171-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2225613-A4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2225613-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8298742-B2 |
priorityDate | 1979-03-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 91.