http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EA-032320-B1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_18a8284bc1d41fe092e46c249d6220be |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-10 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C45-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-10 |
filingDate | 2013-10-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ac704e4c65d8f777d599e35c705871be |
publicationDate | 2019-05-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EA-032320-B1 |
titleOfInvention | POLYETHYLENE COMPOSITION CONTAINING POLYPROPYLENE, METHOD FOR ITS PREPARATION, ITS APPLICATION AND CONTAINING ITS PRODUCT |
abstract | The invention relates to compositions containing linear low density polyethylene, characterized by a mass flow rate of the melt according to the definition when using ASTM D-1238 (190 ° C / 2.16 kg) in the range from 4 to 125 g / 10 min, or high density polyethylene characterized by the mass flow rate of the melt according to the definition using ASTM D-1238 (190 ° C / 2.16 kg) in the range from 4 to 125 g / 10 min, and polypropylene, where the amount of polypropylene is from 0.005 to 10 wt.% when calculating the total linear poly mass low density polyethylene or high density polyethylene and polypropylene, where polypropylene has a melting point (T) in the range from 40 to 200 ° C and / or a crystallization temperature (T) in the range from 100 to 140 ° C, where the values of T and T are determined by using differential scanning calorimetry in accordance with ASTM D 3418-08 using a scanning speed of 10 ° C / min for a sample of 10 mg and using a second heating cycle. The invention also relates to the use of said composition in (thin-walled) injection molding. |
priorityDate | 2012-10-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links