abstract |
The present invention relates to a method for producing clinker based on calcium sulfoaluminate (belite, ferrite, ternesite), comprising the following steps: providing raw meal containing at least sources of CaO, AlO, SO, sintering raw meal in a furnace at a temperature in the range of 1100 -1350 ° C to produce clinker, cooling the clinker, while before sintering or during sintering, a flux / mineralizing additive is added to the raw meal, including at least a glass powder or a mixture of glass powder and compounds containing copper copper The claimed invention also relates to a method for producing calcium sulfoaluminate cement and a binder containing this cement. |