Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8fef08187ee55d4390f40bc12380ddd0 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2333-20 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-215 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F1-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-54 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-18 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-215 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F1-07 |
filingDate |
1980-03-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4f821e19c5b93d2f6e22b00b378cec18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_119330a0ef955bed5f47370e973cfdd3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e331f3cf42aa8d27294c376325095e68 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ac3eb7506b0c7a7fc605d240cd0385ed http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5493886fa2dcbb0ddf747898aceed5f4 |
publicationDate |
1980-09-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
DE-3008753-A1 |
titleOfInvention |
METHOD FOR PRODUCING MODACRYL FIBERS WITH HIGH GLOSS, HIGH HEAT STABILITY AND HIGH FLAME RESISTANCE |
priorityDate |
1979-03-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |