Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0193de021ad7b75a9fef2b4727c66d83 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C2217-229 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C2218-32 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C17-23 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C21-002 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C17-25 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C17-23 |
filingDate |
1976-02-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c16d86f0e0b3577da9e99e50c1163433 |
publicationDate |
1976-10-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
DE-2605883-A1 |
titleOfInvention |
PROCESS FOR CHEMICAL INCREASING THE BREAKING STRENGTH OF GLASS ARTICLES |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-3840071-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5127931-A |
priorityDate |
1975-04-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |