abstract |
Lithium vanadium oxide having a specific surface area of 0.5 to 50 m 2 / g, preparable by a process comprising the steps: a) Preparation of a solution or suspension of water, at least one water-soluble lithium salt, at least one water-soluble vanadium compound and optionally further components, wherein at least the lithium salt and the vanadium compound are also completely dissolved in the suspension, b) drying the solution or suspension prepared in step a), and c) calcination of the solid obtained in step b). |