http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-19914708-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d7b8bf13118bb6b8e78ae7752357a51b |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F16C13-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21G1-0233 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21G1-02 |
filingDate | 1999-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8ee7b85812bd5f6b454a4be07461dcee |
publicationDate | 2000-10-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | DE-19914708-A1 |
titleOfInvention | Roller, in particular for smoothing paper webs, and method for producing such a roller |
abstract | A method for producing an elastic roller with a hard roller core, in particular made of metal, and an elastic reference layer is described. In the method, to form the reference layer, a radially inner connecting layer is wound on the roller core and then a radially outer functional layer on the connecting layer and / or the functional layer simultaneously glass fibers and carbon fibers are wound on the roller core, the mixing ratio of glass fibers to carbon fibers between approx. 60 / 40 and 90/10, preferably 70/30. A corresponding roller is characterized in that the inner connecting layer and / or the outer functional layer consists of a mixture of glass fibers and carbon fibers which are embedded in a soft matrix material and are in each case essentially uniformly distributed over the length of the roller. The mixing ratio of glass fibers to carbon fibers is between approximately 60/40 and approximately 90/10, preferably approximately 70/30. |
priorityDate | 1999-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |