abstract |
Use of a thermoplastic molding composition other than ABS, containing, based on the sum of the amounts of components A, B and C and, if appropriate, D and E, which gives a total of 100% by weight, DOLLAR A a: 1-48% by weight at least a single- or multi-phase particulate emulsion polymer with a glass transition temperature below 0 ° C. of at least one phase and an average particle size of 50-1000 nm, preferably 50-500 nm, as component A, DOLLAR A b: at least 1-48% by weight an amorphous or partially crystalline polymer as component B, DOLLAR A c: 51-98% by weight polycarbonate as component C, DOLLAR A d: 0-47% by weight of conventional additives and / or fibrous or particulate fillers or mixtures thereof Component D and DOLLAR A e: 0-5% by weight of at least one low molecular weight halogen-free acid as component E, DOLLAR A as a swelling-resistant molding compound for the production of body parts and their semi-finished products for motor vehicles. |