http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-19816591-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_654d63da3d02b907b4c87d1c9eba71a6 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K3-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A01K1-0154 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A01K1-0155 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A01K23-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A01K1-0152 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K3-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J20-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A01K23-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J20-22 |
filingDate | 1998-04-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3b199849bbc00ac49d7e04d99455e8db |
publicationDate | 1999-10-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | DE-19816591-A1 |
titleOfInvention | Light clumping small animal litter and process for their production |
abstract | The currently offered clumping small animal litter made mainly of mineral raw materials has bulk weights of up to 1.2 kg / liter, which is disadvantageous for the consumer. The relationship between the suction power and the clumping effect is not optimal. The small animal litter according to the invention should therefore be slightly clumping DOLLAR A È with a low bulk density (400-480 g / liter) and a yield when mixed with water (liquid animal excrement) of less than 50 g small animal litter per 50 ml water added within a period of 8- 10 sec, DOLLAR A È achieve good odor retention and are largely dust-free, DOLLAR A È are manufactured using and using frequently available, inexpensive raw materials and their effective processing. DOLLAR A According to the invention, the small animal litter consists of DOLLAR A È 42 to 96% shredded waste paper, DOLLAR A È 2-8% water, DOLLAR A È 1-30% blue and waste bentonite, DOLLAR A È 1-20% anhydrite binder, DOLLAR A È one Envelope made of bentonite in a ratio by weight to dry waste paper of 0.8: 1 to 2: 1. DOLLAR A The invention relates to the components of an animal litter as an absorbent for animal excrement and a process for their production. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-03022387-A2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-03022387-A3 |
priorityDate | 1998-04-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 36.