http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-19816460-C1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e4984750b19edaace92595210f98bedc |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2325-04 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-224 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-224 |
filingDate | 1998-04-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1999-12-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_380e29a579531d3c6494e6ed3771521d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c1e27d4b8ed10b8bafb4d6a32c2a3853 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b9bb1c557b9eb52e918492e3ff9b5cb0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2c749afb5443591da8ba9e6decb76949 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fcaec9fb44a5c48a17400e72ad6d3647 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dd02cb54b16c87dccd50096e75361267 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_587a182d552b95d48f4182badbc69bbd |
publicationDate | 1999-12-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | DE-19816460-C1 |
titleOfInvention | Process for coating expandable styrene polymers |
abstract | With the method according to the invention, it is possible to precoat EPS beads which, even with a very narrow grain size distribution curve with a grain fraction of the main fraction up to 50-70% and / or with a comparatively high fine grain fraction, classify without electrostatic charging and significant mechanical Defect formation on the surface enables. At the same time, it should be ensured that lump formation is also prevented during the pre-foaming process and that the pre-foamed beads in the finished foam have good welding to one another. This is achieved by adding a coating agent as an aqueous slurry of at least two water-insoluble inorganic components and a water-soluble surfactant to the expandable styrene polymer during the solid-liquid separation, the mean particle diameter of the one component being at least a power of ten of that the other component. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2058361-A1 |
priorityDate | 1998-04-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 57.