Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_63ff67fef78b2298c270cc8f6eef148f |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61K2800-412 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21C9-007 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21D1-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61K8-731 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A23L29-262 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61Q19-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21H11-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A23L33-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A23L33-22 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21C9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A23L29-262 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A23L1-308 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61K8-73 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H11-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61Q19-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21D1-30 |
filingDate |
1995-01-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2006-01-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3d24b0fec3aace18da7b8379c9d60d4a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6a82c9f26b8c492cf1987b1b7ae261f9 |
publicationDate |
2006-01-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
DE-19500249-B4 |
titleOfInvention |
Process for the preparation of micro-classified cellulose |
abstract |
methodnfor the preparation of microclassified cellulose (MDC), in whichnyou repeat a liquidnSuspension of fibrous cellulose through a high shear zone,nthe two oppositensurfacesnis formed, with opposite rotation of the surfaces to each other,nwherein the conditions and time duration are chosen such that a substantiallynstable suspension results and this suspension a freenessnwithin the meaning of the Canadian Standard, which isnDecrease to values below 100 a steady increase in repeatednPassage of cellulose through the high shear zone shows. |