Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5cbf16dde85354a090ffad4512af7eaf http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8e26b3a108aa777381140e0777768f2f |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-06 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-3003 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-09 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C48-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C48-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C48-09 |
filingDate |
2003-02-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_71137c37ab756605b81334a6beae4097 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6ec40312c81806c3b1e5242863cd96d2 |
publicationDate |
2004-09-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
DE-10308909-A1 |
titleOfInvention |
Process and extrusion die for eliminating surface melt fractures in the extrusion of thermoplastic polymers |
abstract |
Method and device for substantially eliminating surface melt fractures during the extrusion of thermoplastic polymers such. B. Molten linear low density polyethylene by using a nozzle which has an elastic coating on its inner surface following the nozzle outlet. |