http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-102019206559-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c9555ad31b2c10a5c2c0bc283d03579b |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C10M2217-041 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G73-1032 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G73-1085 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C10M149-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D179-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G73-1082 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G73-1007 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G73-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D179-08 |
filingDate | 2019-05-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_35f457238345259f60ef12b8eff5da8b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_231050433a7ae0f6b385ac665355155c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6348ee29f6ae97d93bf8040134d604c2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3127502e0e33e8e38496b18a700f3c2b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9627913f89ab89cbc52448e0e91a09ab |
publicationDate | 2020-11-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | DE-102019206559-A1 |
titleOfInvention | Imide composition and protectant composition with the imide composition |
abstract | The present invention provides an imide composition obtainable by a method comprising the steps of: a) Reacting a dianhydride with a diamine in the presence of a solvent at a temperature in the range of 20 - 80 ° C, the molar ratio of dianhydride (A) to diamine (B) in the range between 0.25 - 4 (A / B) lies, thereby forming an imide precursor; and b) exposing at least part of the imide precursor, which is formed in step (a), in the presence of a solvent to a heat treatment carried out at a temperature in the range between 80-150 ° C to convert at least part of the imide precursor into an imide to convert, thereby forming the imide composition. The invention also provides a protectant composition comprising the imide composition; a metal article having a coating thereon, the coating comprising the present protectant composition; the use of the present imide composition to prevent and / or reduce corrugation in a rolling bearing system; and the use of the present protectant composition to prevent and / or reduce corrugation in a rolling bearing system. |
priorityDate | 2019-05-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 58.