http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-102015113897-B4
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_62e83a4c9be08118c122809379311900 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-63448 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-63488 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-6342 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-63416 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-111 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B26-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-622 |
filingDate | 2015-08-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-06-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9b85dbba2a7a73a107939330003dbb5e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f40f1429997e97325b00a1c0f741f2e9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bf3b0c18115c3f4f432b7c860fba5da0 |
publicationDate | 2017-06-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | DE-102015113897-B4 |
titleOfInvention | Process for producing a binder matrix for an inorganic, in particular ceramic, solid particle material |
abstract | Method for producing a binder matrix containing at least one binder material and at least one plasticizer material for an inorganic, in particular ceramic, solid particle material, characterized by the following steps: Providing at least one binder material, wherein a binder material is used which is formed as a chemical substance having at least one alcohol group or at least comprises a chemical substance having at least one alcohol group, wherein a polyvinyl acetal is used as the binder material, Providing at least one plasticizer material using a plasticizer material which is formed as a chemical substance having at least one oxygen atom or comprises at least one chemical substance having at least one oxygen atom, wherein at least one diester compound is used as the plasticizer material, Preparing a mixture by mixing the binder material and the plasticizer material at a certain mixing temperature, the mixture having certain optical properties, Cooling the mixture from the determined mixture temperature and detecting a critical temperature at which a change of at least one optical property of the mixture occurs, wherein a change of the at least one optical property of the mixture is a clouding of the mixture or the beginning of a turbidity of the mixture, - Use of the mixture as a binder matrix for an inorganic, in particular ceramic, solid particle material, provided that the detected critical temperature is below a predetermined reference temperature. |