abstract |
The invention relates to a method for producing a dental ceramic milling disk, comprising the steps of: providing (100) or producing (101) a first slurry (10); Pressure filtering (102) the first slurry (10) in a separation device (1) having a filter means (6, 22) with a maximum pressure differential of 200 kPa or more such that a filter cake (12, 20) is attached to the filter means (12). 6, 22) is deposited; Removing (104) the filter cake (12, 22) from the separation device (1); Drying (106) of the filter cake, so that a Frässcheiben-green body is formed. In this case, the first slurry (10) comprises a first solid phase and a first liquid phase, wherein the first liquid phase comprises water and the first solid phase consists of a first ceramic powder, and wherein the proportion of the first solid phase to the first slurry (10 ) at the beginning of pressure filtration (102) is at least 10% by volume. |