http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-102007051684-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1ac5971487f616fc6e63ec3edefcb6dd |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C2218-112 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C17-3623 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C17-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C17-3663 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C17-3618 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C17-36 |
filingDate | 2007-10-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_54609ed0ee3eebaac4cf7cfc7d43507d |
publicationDate | 2009-05-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | DE-102007051684-A1 |
titleOfInvention | Method and means for producing copperless mirrors |
abstract | A process for the production of copperless mirrors with a reflecting layer of silver deposited on glass plates, characterized in that a solution of stannous chloride in an organic solvent such as. B. alkylene glycols and their mono-alkyl ethers and polyalkylene glycols and their mono-alkyl ethers are metered into a stream of demineralized water and sprayed onto the silver layer. As a result, a very effective corrosion protection layer is formed, without the adhesion between silver and glass is weakened in contrast to acidic tin (II) chloride solutions according to the prior art, which are used to form a corrosion protection layer. |