http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-102007030672-B4
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ef5f2d6e752482922ca30c6fc6d48be1 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B27K3-15 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B27K3-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B41-4922 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B41-009 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B41-49 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B41-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B27K3-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B41-49 |
filingDate | 2007-07-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-05-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-05-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | DE-102007030672-B4 |
titleOfInvention | Process for preserving porous substances |
abstract | Method for preserving porous substances in the form of objects made of stone or wood with a liquid mixture by impregnating the porous material with organoalkoxysilane and subsequent drying, wherein the mixture contains at least two substances from the group of organoalkoxysilanes, wherein a substance of the mixture is an organoalkoxysilane containing at least one epoxide unit, and wherein a substance of the mixture is an organoalkoxysilane containing at least one amine function, and wherein the mixture to initiate the hydrolysis, an appropriate amount of water is added, the water is added just before soaking, without affecting the penetration in the required penetration more negative. |