http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-102005043865-B4
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_daeceae3e45bdccd3d2adef271c842a9 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P70-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E10-542 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G9-2031 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D11-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D11-024 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D11-026 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y30-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D11-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82B3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L31-06 |
filingDate | 2005-09-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2014-01-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e52f8947580bf3c840bcd73ec2689eb5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1d656c6811510a9fee31f3c83a428052 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5839bc5aeb6a2ee8ca72e9dfcf654330 |
publicationDate | 2014-01-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | DE-102005043865-B4 |
titleOfInvention | Process for the preparation of nanocrystalline or nanocrystalline metal oxide and metal mixed oxide layers on barrier layer-forming metals |
abstract | Process for the preparation of nanocrystalline or nanocrystalline metal oxide and metal mixed oxide layers on barrier layer-forming metals, in which a substrate to be coated is cleaned and degreased anodically an aqueous electrolyte containing one or more complexing agents in the concentration range 0.01-5 mol / l, one or more Metal alkoxides or suitable derivatives of these compounds in a concentration greater than 0.01 mol / l and alcohol in a concentration greater than 0.01 mol / l contains, in the electrolyte anodization process under spark discharge with DC voltage or DC pulses and temporal change of the voltage to takes place at a final coating voltage and in which the coated substrate is rinsed from the electrolyte for cleaning and then dried, characterized in that the electrolyte at least one further organometallic compound and / or an organometallic in a Konze ntration is added less than 0.01 mol / l. |
priorityDate | 2005-09-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |