Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a2bcaf91101a370a3d64e3190366357f |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K3-3463 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B23K35-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B23K35-262 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05K3-34 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23K35-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23K35-26 |
filingDate |
2001-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_89d2b7d38ffb9abaf9e0253ede2eed03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6f917ae5bb53be463ceb169ca4d3a151 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d07d6e910b62702bcd6ff7dd46c8705e |
publicationDate |
2002-10-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
DE-10115482-A1 |
titleOfInvention |
Solder composition and method of making the same |
abstract |
A solder composition consisting of a starting solder composition and at least one alloy component is described. DOLLAR A The invention is characterized in that the alloy component consists of a metal or several metals with a melting temperature above 750 ° C. and that the starting solder composition is based on a metal with a melting temperature below 430 ° C. Manganese (Mn) and / or iron (Fe) are particularly suitable as alloy components. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-10304469-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8823245-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-102009054068-A1 |
priorityDate |
2001-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |