Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_520278049ae6d5edd47f3440abdc5a27 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B5-021 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B5-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B5-225 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C1-004 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03B5-235 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03B5-225 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03B5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03B5-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03B5-02 |
filingDate |
2000-01-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2006-03-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b65e3e3758520bd631c225b610ec1612 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_03e1dab54f115c2c03fb247a619d4678 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_da689ef46fbde4d7a220e494279afaff http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_42478cdead391c4975620fe4ec7295f8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_361b8ca21d1eda5b2d7f876ebca9bf8d |
publicationDate |
2006-03-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
DE-10003948-B4 |
titleOfInvention |
Process for melting, refining and homogenizing molten glass |
abstract |
Method for producing a glass melt 1.1 with a melting step; 1.2 with a lauter step; 1.3 with a platinum homogenizing and conditioning stage 1.4 wherein prior to the homogenizing and conditioning stage, the melt is heated to a temperature above 1700 ° C; 1.5 wherein in the melt polyvalent ions are present in a proportion of at least 0.5 wt .-%. |