http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DD-278130-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_805609fba7e9ac33795d126769c88b7d |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C23-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23K26-00 |
filingDate | 1988-12-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_45cb41dc4c3c4fb404e0600a4a1dee31 |
publicationDate | 1990-04-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | DD-278130-A1 |
titleOfInvention | METHOD FOR LABELING GLASS TUBES |
abstract | The invention relates to a method for labeling glass tubes, as z. B. in the glass industry for applying scales and characters on measuring tubes, Schauglaeser, level gauge u. ae. is applied. As the absorption layer is on the pipe to be inscribed a resistant fusing color with a temperature resistance between 327 K and 627 K used, which is treated in the dried state with a laser beam of a power between 20 W and 30 W together with the glass tube. The laser beam operates for a period of time between 0.03 and 0.06 seconds in cw mode on each point of the intended labeling line until the glass cylinder is brought into a ready-mix viscous state at the respectively applied point and a surface connection between color and glass has occurred , |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-10259006-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-102014219480-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-4022745-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2010057470-A2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-102008058556-A1 |
priorityDate | 1988-12-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 21.