http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DD-250289-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b026b0f817cbe042d7639c26b86b10c4 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B27K5-00 |
filingDate | 1986-06-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_18349971cc206b153d7b4f94f7d581ba http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_09c5c6b9d14941e4c043d364c2826f5a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_94bcabf4d4749d47b0cdd11a78d5eab8 |
publicationDate | 1987-10-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | DD-250289-A1 |
titleOfInvention | PROCESS FOR THE FURNISHING AND REFINING OF OBJECTS OF WOOD OR SIMILAR MATERIAL |
abstract | The aim of the invention is to develop a method that is equally applicable for articles made of wood or similar materials and for all types of wood, with low cost high profitability and good usability properties secures, is environmentally friendly and impraegniertem wood or similar materials, the free Contain formaldehyde, which eliminates health risks. The invention shows a solution which is used for all types of wood or similar materials based on the colorants contained in wood, without Vorbeizung and additives, at a room temperature of about 20C, almost under cell conditions, without pressure, with gaseous ammonia in high concentration can be, and which concludes with the subsequent refining by means of polymerizing liquids at normal room temperature and without application of pressure. In the process, the natural wood structure is preserved, refined or particularly emphasized by the positive pickling pattern. At the same time, excellent utility value properties are achieved, which can not be reduced. a. in color fastness and in a certain protection against chemical and physical influences. In the case of imprained wood or similar materials, the pollutant emission is minimized by the binding of the free formaldehyde so that the ambient air concentration meets the international standard. The method is suitable for items made of wood or similar materials in the furniture industry, the woodworking industry, the tool and household goods industry, the cutlery and cutlery industry, in the arts and crafts as well as in the interior and exterior architecture. |