http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DD-156169-A1

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_30d8849cf07775cbcf2c851353863aa2
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_fb1edbe3e71fc8d974ec4246ee1f3d5c
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2556431b96ef4f17faad7f10e39547d8
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_54bdf50118324a0b1eadf5d5d6584523
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5926319a056de93163643b3f4a84361d
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4c9d294c097d5f80f992bf6d59d46b6a
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2f3413a6b9b355ade124faa9512d4d97
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_65daab3dcf10f710041017500a8e9db9
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-755
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-755
filingDate 1981-02-05-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4fb4f27cefc1de1c70d681cfc802f04e
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e62f2d3c1169f55f291c5d11d3682f29
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e7eadcf7c24b371e45c06d6864645844
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8ef5a4f7fe030d1cbe7a5d73298592fe
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_57b4c7a9e7b8c82523a78f5486303865
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_560523b845c1e4878cd691cda2dc1209
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_24fb73cea24b45737d7c98cc49a49f67
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1198dfe7859ec20a6f5103c3990709d8
publicationDate 1982-08-04-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber DD-156169-A1
titleOfInvention PROCESS FOR STABILIZING PYROPHOROUS NICKEL ALUMINUM OXODY CATALYSTS
abstract The invention relates to a method for stabilizing pyrophoric Ni-Al deep 2 O deep 3 catalysts. The aim of the invention is to find a new method for stabilizing Ni-Al deep 2 O deep 3 catalysts, according to d. stable, storable u. activatable catalysts are produced. The essence d. Invention is d. Ni-Al deep 2 O deep 3 catalysts are treated with inert gas after reduction at least at reduction temperature for a certain time until complete hydrogen desorption; After cooling from 383 to 353K air in d. Inert gas stream dosed until the exhaust gas 1 to 5% by volume of oxygen
priorityDate 1981-02-05-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID43677
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID425193155
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID413956194
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID783
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419523291
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419526493
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID977
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID61739

Total number of triples: 33.