http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DD-151602-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d6056a76016b20054aeaf097183d0916 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0b0936bf1ede98d160793383fe86a7af |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C37-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22C1-16 |
filingDate | 1980-06-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_29770a3b9fdee7835e836d217116c99c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a6bd4073f0e4cf5b170b5516047d7cd3 |
publicationDate | 1981-10-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | DD-151602-A1 |
titleOfInvention | METHOD FOR THE PRODUCTION OF IMPACT STRIPS FROM CAST IRON |
abstract | The invention relates to a method for the production of blow bars made of alloyed, white solidified, wear-resistant cast iron, in particular for impact crushers and -muehlen for the crushing of hard rock. The aim and object of the invention is to produce blow bars without mechanical processing so that the demands made on the machines with respect to imbalance erfuellt. According to the invention, the object is achieved in that a material in the chemical composition C 2.8-3.2%, Si 0.8-1.1%, Mn 1.8-2.2%, P <0.40 %, Cr 11.5-13%, Mo 1.8-2.3% and Ti <equal to 0.20% in horizontal forms and / or as a core block, consisting of the molding material system quartz sand, water glass 48 degrees Be, bentonite, bauxite and aluminum stearates is shed. The invention is applicable to wear-resistant parts, since the treatment takes place in dependence on the Gusskoerperquerschnitt and subsequent processing is avoided. |
priorityDate | 1980-06-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |