Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4fe394cc69f1a5ac343cd870c11fc65d |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F212-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L25-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-20 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F212-36 |
filingDate |
2014-06-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5de33dd266903ebfd3d199463f1bfc08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8263c6abb4dccb252a8910670649fc2b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6e57c5515ef9e9d95a7a9d51818ce09e |
publicationDate |
2019-10-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
CZ-307994-B6 |
titleOfInvention |
Styrenic polymer and process for its preparation |
abstract |
Styrenic polymer in the form of spherical particles with a mesoporous morphological structure with an average pore diameter of 10 to 100 nm and a pore proportion exceeding 60% of the volume of the spherical particles. The process for preparing the styrenic polymer is carried out by suspension radical polymerization from a monomer mixture comprising at least one styrenic monomer capable of forming cross-linking bonds and a water-immiscible solvent and capable of swelling the styrenic monomers in a volume equivalent to two to ten times the volume of monomer. |