Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b8be6a6c990669567cc455d32b00535e |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F8-50 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-10 |
filingDate |
1997-06-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f78bc1dc7f791f9140aae520b46669de http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_837ec79d5f74886e298b17401b426e1b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3583ed17e7493ee75c62b78034d90dd4 |
publicationDate |
2003-04-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
CZ-291628-B6 |
titleOfInvention |
A method for increasing melt strength |
abstract |
The method of increasing the melt strength of polypropylene (co) polymer by means of initiator dispersions. To use a dispersion of the initiator to initiate the initiator in a non-dispersed state or solution or solution leads to a significant increase in the melt strength of the modified polymer, and possibly to a range of initiators. . |
priorityDate |
1996-06-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |