http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CZ-282773-B6
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e7e43836ed06e39d03fffbe4b448319e http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f3e450e3e4ec97dbaea8ab20612e0a33 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D53-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D53-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D53-64 |
filingDate | 1993-01-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_974a2b4bb81cf79d5ea63cb05a63eac7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_12c7b3087db8ae4eb4caa96c0d4f664e |
publicationDate | 1997-10-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CZ-282773-B6 |
titleOfInvention | Coal desulphurisation method |
abstract | Desulphurization of the coal to be combusted is accomplished by the addition of calcium oxide powder in an amount of 60 parts by weight. of calcium oxide to 3,000 parts by weight; coal. In order to reduce the total exhalation of coal combustion, in particular the release of heavy metals in the form of oxides, additional water glass is added to the pre-treated calcium oxide with an amount of 40 parts by weight. of water glass to 3,000 parts by weight. coal |
priorityDate | 1993-01-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |