http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CS-266770-B1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_87af6a86295fbb59fa720403d4cd7254 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_bf523d96b6989f154e795a65a04cd119 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B25-44 |
filingDate | 1988-06-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a259486c5ba57247edfcf24c5aa33bc0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dbcc631ea83fcb9aaa57e3136bff04db |
publicationDate | 1990-01-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CS-266770-B1 |
titleOfInvention | A high temperature process for the preparation of cadmium-magnesium double cyclo-phosphates |
abstract | The method consists in calcining the starting materialnmixtures consisting of cadmium compoundsnand magnesium-type dihydrogen phosphates,nresp. acid mixturesnphosphorous with hydrogen phosphatesnor cadmium phosphates anwith magnesium, or with oxides, hydroxides,ncarbonate hydroxide or carbonatesnand feverishnin amounts corresponding to molarnratio Cd / Mg = (2-x) / x anPpOc / tCd + Mg) equal to 0.98 to 1.15,nto temperatures above 800 ° C, whenna melt is formed. The one is sharpnby cooling it to a vitreous intermediate,nwhich is heated by heatingnto a temperature of at least 500 ° Cnand less than 750 ° C is recrystallizednto form double-microcrystalsnCyclo-tetraphosphatenemnato-magnesium. |