http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CS-229065-B1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8c827738ca17bd799d55028e52c8501e http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_256ed7334a45ec550b20f45852ae25ed http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_212cb5a1869be04fdfb4f700893aacc9 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-06 |
filingDate | 1981-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cfa43c12cb8601e051b17dcfa2a88f6d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_562f482203c9dee23e6733ed25362b50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_df9916962f16d4359a4f24b35168807b |
publicationDate | 1984-05-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CS-229065-B1 |
titleOfInvention | A method of preparing polypropylene cable fibers using their hard wastes with improved properties |
abstract | A method for producing polypropylene cable ductsnfibers when using their hard wastes,nwhich can be from compact tonstrunove.nThese wastes are crushed in a crusher,n600 and over 600 kg / hn45 and below 45 kW, and so preparedngrit 8 melt index 3.5 to 17 gnfor 10 min, preferably 3.5 to 9 g / 10 min,nis added in an amount of up to 15, preferably ton3% polymer-based and mixed with the originalngranular polypropylene; \ tor. \ tnwith a pigment concentrate or part thereofnsaid amounts of pulp are mixed with the polymernand another portion of the pigment concentratornand the resulting mixture is spun at temperaturesn220 DEG-325 DEG. |