http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-215800396-U

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_de9537f3f0055b7e46b980f857f98bb4
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06B23-22
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06B23-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06B15-09
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06B3-04
filingDate 2021-07-23-04:00^^<http://www.w3.org/2001/XMLSchema#date>
grantDate 2022-02-11-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_03e421f8fb88fc5ab1fb0e1e229dd8fb
publicationDate 2022-02-11-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber CN-215800396-U
titleOfInvention Low-temperature energy-saving glue dipping production line for pipe glue line
abstract The utility model discloses a low-temperature energy-saving impregnation production line for a pipe rubber line, which comprises a paying-off mechanism, an impregnation mechanism, a drying mechanism and a winding mechanism, wherein the pipe rubber line sequentially bypasses the four mechanisms, the drying mechanism comprises a horizontally arranged oven, three layers of horizontally extending channels are arranged in the horizontally arranged oven, the drying channels, the middle channels and the heating channels are respectively the uppermost layer of the drying channels, the drying channels and the middle channels are separated by first partition plates, a second partition plate is arranged between the middle channels and the heating channels, a plurality of through holes are formed in the second partition plate, an air inlet fan is arranged at one end of each middle channel, and a natural gas combustion head with adjustable flow is arranged in each heating channel. The production line provided by the application simplifies the structure, reduces the drying temperature, is beneficial to saving energy, and is low in cost and more environment-friendly; the rubber thread surface control device is used for drafting through the drafting roller, gum dipping is carried out after the drafting, then the rubber amount on the surface of the rubber thread is controlled through the rubber amount control roller, the gum dipping quality can be effectively improved, the smoothness of the surface after gum dipping is guaranteed, and the quality is improved.
priorityDate 2021-07-23-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID422074910
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID13738549

Total number of triples: 16.