http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-209438405-U

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8db4922481b332b925da94a99217e722
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D53-50
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D53-80
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01F7-00
filingDate 2019-01-10-04:00^^<http://www.w3.org/2001/XMLSchema#date>
grantDate 2019-09-27-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_299aef156335a98c901a495986a76bac
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4a9390208860fea180a557a4112cb021
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_36f9a90169e8804797c94bc026bb3c37
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_69f9653c5559901307e62acdd0b3d45a
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f139a5b20cfd318896a9738cafdb2cf2
publicationDate 2019-09-27-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber CN-209438405-U
titleOfInvention A kind of silicon-carbide metal cast structure part
abstract The utility model discloses a kind of silicon-carbide metal cast structure parts, belong to desulfurization technical field of environment protection equipment.The silicon-carbide metal cast structure part, including metal body and the silicon carbide wearing layer for casting in metal body surface.Wherein, the metal body include at least two panels blade and connect blade power shaft connection mechanism;The through-hole of perforation two sides of blade is equipped on each blade.The axial direction of through-hole is not vertical with plane where blade.The structural member opens up the through-hole structure that certain tilt angle is formed with casting face on the casting face of metal body, and the contact area of the cast material and metal body that are on the one hand filled into inclined hole increases, and connectivity robustness improves;On the other hand, in the structural member after casting in whipping process, the stress of through hole be will disperse on metal body, and through hole can effectively be avoided to become damageable zone.
priorityDate 2019-01-10-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID9863
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419549006
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID450711093
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID26268
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID448976021
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID10154041

Total number of triples: 23.