http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-207713670-U
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0788e226c1e91db4369bbd7711c796bd |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J163-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-04 |
filingDate | 2017-08-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-08-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_402986244c406be256c3d7c4e4f1c32e |
publicationDate | 2018-08-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-207713670-U |
titleOfInvention | A kind of composite plate |
abstract | The utility model discloses a kind of composite plate, including the first composite layer, the second composite layer, first composite layer is connected by adhesive layer with the bonding of the second composite layer;The adhesive layer is melted by the heating of one-component epoxy resin rubber powder.A kind of composite plate described in the utility model, the setting of adhesive layer not only improves the bonding strength between composite layer, but also can improve the glued stability of composite layer, to improve composite plate whole service life. |