http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-206483453-U

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d6a6f422b091ba12ea61d4adbf1b0e8e
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D53-72
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-34
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D53-86
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J37-34
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J19-08
filingDate 2017-01-22-04:00^^<http://www.w3.org/2001/XMLSchema#date>
grantDate 2017-09-12-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_47f97c8898a8b6cd1fcec3941833dd45
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2c39ca9a94f0e48a9a87bcf90c633751
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_67fc6bf06373d11a9c7e2868aa42621b
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_867326248dcfd99b3c9b9c160ec482fd
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8fdb8483dbb5514378622832f79461f5
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_657a44b7ee23c084478e621629b53612
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_81ee15071a033efcaf749eb62b621010
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e8634c0ea4aad56c55c54dda5f0005ec
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c7d9f2f133c68ba69240cc11b9de3bda
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_10510e50a667bb3bf19134343b1c7364
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_54425c0a8bffefa36cb6c1fd55cd86e9
publicationDate 2017-09-12-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber CN-206483453-U
titleOfInvention A kind of low-temperature plasma modified catalyst device
abstract The utility model is related to a kind of low-temperature plasma modified catalyst device, described device includes quartz ampoule, high-field electrode and grounding electrode, high-field electrode is connected by polytetrafluoroethylene (PTFE) set with quartz ampoule, grounding electrode is wrapped in quartzy tube outer surface, connect with ground wire, the high-field electrode is a stainless steel bar for being placed on quartz ampoule axis, and it is connected with high-frequency ac power;The region of discharge of quartz ampoule is filled with catalyst.Catalyst packing is modified in low-temperature plasma modified catalyst device with easy to operate, flow is short, it is easy to accomplish automatically control, and stability is good, is that a kind of used time is short, temperature is low the advantages of cleanliness without any pollution, the small technique of energy consumption;The better catalytic activity of modified catalyst in the utility model device, modified catalyst has higher methyl sulfide catalytic oxidation activity, and 360 DEG C of the catalysis oxidation efficiencies reach as high as more than 90%;The utility model facilitates production application, with higher industrial application value.
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109675560-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106693854-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106693854-B
priorityDate 2017-01-22-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID61511
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID1068
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID449477149
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID457707758
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID24261
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419539309
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID458393800
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID450868169
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID24948

Total number of triples: 37.