http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115197611-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_781efc7f6a39698a62bb7bce44b84267 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2296 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-162 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D125-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-45 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-47 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-65 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-63 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-47 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-45 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-65 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-63 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D125-14 |
filingDate | 2022-08-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4b7a12f6c9f4a0cb09106c4e0eb45cef |
publicationDate | 2022-10-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-115197611-A |
titleOfInvention | A kind of water-based red rubber waterproof coating and preparation method thereof |
abstract | The invention discloses the technical field of waterproof coatings, in particular to a water-based red rubber waterproof coating and a preparation method thereof. Each component is measured according to mass percentage: 30-40% of styrene-acrylic emulsion, 10-15% of calcium powder, and silicon-acrylic emulsion 10-20%, barium sulfate 10-20%, water 5-10%, iron red powder 2-5%, film-forming agent 0.5-1%, anti-settling agent 0.2-1%, step 1: each component raw material according to The proportions need to be weighed and stored separately by utensils; Step 2: First add water to the reaction kettle, then add the emulsion, dispersant, silicone-acrylic emulsion, iron red powder, calcium powder, wetting agent and defoaming agent in turn. It is added into water and uniformly stirred by a stirring device. The beneficial effects of the present invention are as follows: the water-based red rubber waterproof coating product of the present invention is an environmentally friendly high molecular polymer elastic waterproof material, the product is non-toxic and tasteless, and has good adhesion. It has strong adhesion to mortar cement base stone surface, stone and metal products. The product has stable performance and can withstand sunlight for a long time. |
priorityDate | 2022-08-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |