http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115141582-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9eda26facf50f262ff525627064187c2 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F218-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J131-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F222-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F218-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F218-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J131-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-18 |
filingDate | 2022-06-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0553469d2c3f8ef8cf2245dff5f70f24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8f5daa6128dff2212ff24674799ee8dd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0203233579f69e11d45ff17b91e60974 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_963497e0872b54f51f69b2f6dd902d8c |
publicationDate | 2022-10-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-115141582-A |
titleOfInvention | A kind of non-iron jelly-like waterproof veneer glue and preparation method thereof |
abstract | The invention relates to a non-iron jelly-like waterproof veneer glue and a preparation method thereof. The main components and the preparation method are as follows: mixing vinyl acetate, soft monomer, tertiary vinyl carbonate, acrylic acid, functional monomer and internal plasticizer, The monomer mixture is obtained for subsequent use; polyvinyl alcohol, modified polyvinyl alcohol, and deionized water are added to the flask, heated in a water bath, and pH buffering agent, emulsifier and partial initiator are added after cooling down; the monomer mixture and remaining initiator are added dropwise ; Finally, add external plasticizer, defoamer, cross-linking agent and preservative to get veneer glue. The veneer glue prepared by the invention has short initial sticking time, high bonding strength, good roll coating property, strong water/solvent oil resistance, no ironing, and can be repaired; the synthesis process is simple, the raw materials are cheap, and it is suitable for practical application. |