abstract |
The present invention relates to the technical field of thermoplastic resins, and more particularly, the present invention relates to a thermoplastic resin solution and a thermoplastic resin material. The thermoplastic resin solution, in parts by weight, includes 95-105 parts of thermoplastic resin and 78-85 parts of solvent; The solvent includes (a) solvent A with a boiling point of 70-85°C and/or (b) solvent B with a boiling point of 140-170°C. The spun fiber obtained in the application can be peeled off from the carrier well, and the peeling integrity is good, and at the same time, the obtained thermoplastic resin material has good waterproof, breathable, and moisture-permeable properties. |