http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115074025-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6fa25505ca5d0a9187b8ff0f987ea2d5 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2206 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-65 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D183-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-61 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-65 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-61 |
filingDate | 2022-08-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b7d497d68ab4f80c1e4a221d6c4e2e95 |
publicationDate | 2022-09-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-115074025-A |
titleOfInvention | A kind of thermal insulation coating for bomb, preparation method and thermal insulation coating |
abstract | The invention discloses an elastic thermal insulation coating, a preparation method and a thermal insulation coating, belonging to the technical field of coating coating preparation. 20 parts of the organic solvent and 0.5 to 1 part of the coupling agent are mixed uniformly to form a uniform mixture. 1 part to 3 parts of a crosslinking agent and 0.5 part to 1 part of a catalyst are added to the mixture for reaction, and the thermal insulation coating is obtained after the reaction is completed. The thermal insulation coating prepared by using the thermal insulation coating can not only achieve room temperature curing, short curing time, and good interface bonding performance with the substrate; but also has excellent comprehensive performance of high temperature resistance and thermal insulation, which can extend the reaction temperature in the bomb to 17 minutes. , to solve the problems of low reaction temperature of ammunition and short reaction time of ammunition in the prior art, which cause accidents in ammunition transportation or storage and cause economic losses. |