http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114902096-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B7-023 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-29 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J201-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-3083 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-3041 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-30 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B7-023 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-29 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J201-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-30 |
filingDate | 2020-12-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_70a3892a2c0e37bb8c83999e2a2cdfd4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ac61b2e3fd3c8e845b0f1ffe08cf8da3 |
publicationDate | 2022-08-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-114902096-A |
titleOfInvention | Optical Laminate |
abstract | The migration of the dichroic dye from the polarizer becomes remarkable especially in a high-temperature and high-humidity environment. Therefore, even in a high-temperature and high-humidity environment, the transfer of the dichroic dye contained in the polarizer to the conductive layer can be prevented. The resulting deterioration of the conductive layer of the optical laminate. An optical laminate comprising a polarizer, a first cured product layer, a retardation layer and an adhesive layer in this order, wherein the polarizer is formed of an iodine-containing polyvinyl alcohol resin, and the first cured product layer is an active energy curable composition The cured product, the retardation layer contains at least one retardation developing layer of a polymer which is a polymerizable liquid crystal compound, and the iodine content of the adhesive layer after storing the optical laminate at a temperature of 80°C and a relative humidity of 90% for 250 hours When it is 900 mg/kg or less, the polarizing plate and the first cured product layer are in direct contact with each other, and the first cured product layer and the retardation layer are in direct contact with each other. |