http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114891404-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-02 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D127-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F292-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F283-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F212-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F292-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D151-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F283-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D151-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D127-18 |
filingDate | 2022-07-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2022-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2022-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-114891404-B |
titleOfInvention | A kind of antistatic Teflon film and its preparation method and application |
abstract | The invention provides an antistatic Teflon film, a preparation method and application thereof, and belongs to the technical field of polymer materials. , prepare SiO 2 porous hollow spheres, add them to aniline ethanol solution, after reaction centrifugation, add a solution containing Fe 3+ ions to obtain sea urchin-shaped polyaniline-SiO 2 composite hollow spheres, which are placed in metal ion-doped alumina sol Metal ion- doped Al 2 O 3 composite sea urchin - like polyaniline-SiO 2 hollow spheres prepared by reaction in The composite sea urchin-shaped polyaniline-SiO 2 hollow sphere is added with styrene, emulsifier and water, and polystyrene-microsphere emulsion is obtained by polymerization, and after mixing with the polytetrafluoroethylene emulsion uniformly, it is coated with a dip-pulling method to obtain Anti-static Teflon film. |
priorityDate | 2022-07-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 86.