abstract |
The invention discloses a quick-drying cement self-leveling mortar and a production process thereof. ‑60 parts of anhydrite, 3‑5 parts of compound water reducer, 0.03‑0.05 parts of cellulose ether, 0.8‑1.2 parts of lithium carbonate, 1.2‑1.5 parts of defoamer, 0.8‑1.2 parts of tartaric acid, 20‑35 parts of glue Powder, 200‑300 parts of water; sulfoaluminate cement, Portland cement and anhydrite are used as cementing materials, tartaric acid is used as a retarder, and lithium carbonate is used as a coagulant, which can dry quickly after cement self-leveling construction. Reduce the adverse impact on subsequent construction and save labor costs. |