http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114686068-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4716ebd2c85b8f570dc39a3ab62493f0 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-011 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-0812 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-08 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D133-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-103 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-63 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-63 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D171-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-10 |
filingDate | 2022-05-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_da8d3429edee84eb333e8701bad27164 |
publicationDate | 2022-07-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-114686068-A |
titleOfInvention | A kind of protective coating and preparation method thereof |
abstract | A protective coating and a preparation method thereof, comprising the following raw materials in parts by weight: 20-30 parts of nano-silica sol, 15-25 parts of polyethylene glycol, 10-20 parts of talcum powder, 7-12 parts of silica dispersion, 5-15 parts of aluminum silicate fiber, 2-5 parts of dimethylaminopropyl acrylate, 20-30 parts of copper tungstate, 10-20 parts of film former, 1.6-2 parts of dispersant, 4-8 parts of ethylenediamine , 10-20 parts of hydroxyethyl acrylate, 40-50 parts of alcohol amine, 20-30 parts of graphene, 5-10 parts of conductive mica powder, 40-45 parts of aluminum powder, 15-20 parts of ethyl acrylate. The coating prepared by the combination of components and preparation process steps has high gloss, high temperature resistance, high corrosion resistance, strong contact adhesion, high hardness of the coating film, good heat dissipation performance, and is not easy to agglomerate, and is suitable for various metals. , plastic, glass surface treatment, even in high temperature environment also has good comprehensive performance. |