abstract |
The present invention relates to a thermoplastic resin having excellent non-whitening properties while having excellent impact strength, gloss and fluidity, and a method for producing the thermoplastic resin. More specifically, the present invention provides a thermoplastic resin comprising an alkyl acrylate-alkyl methacrylate graft copolymer (A), or an alkyl acrylate-alkyl methacrylate graft copolymer ( A) and a matrix resin (B) comprising a resin selected from the group consisting of aromatic vinyl compounds-vinyl cyanide compounds-alkyl methacrylate copolymers and alkyl methacrylate polymers One or more, wherein the transparency measured under the condition of 3mm thickness is less than 5, the total content of alkyl acrylate is 20 to 50% by weight, and the alkyl acrylate coverage value calculated by the following formula 1 ( X) is 65 or more: [Calculation formula 1] X={(G‑Y)/Y}×100, where G represents the total gel content (%) of the thermoplastic resin, and Y represents the amount of gel in the thermoplastic resin contained in the gel Content (weight %) of alkyl acrylate. |