http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114394794-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c95b4a0e58101e5c92c116cc12ee310a |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2201-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-343 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B20-023 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B20-04 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B111-34 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B20-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B14-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B14-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B20-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-04 |
filingDate | 2021-12-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b969bbea6eee7301c1f2fd35f54fa4ed http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b22d20bbd3b97d767cd9955ac8cd6621 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d6b222315fcfbd2787a0ad06bf27be6e |
publicationDate | 2022-04-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-114394794-A |
titleOfInvention | A kind of preparation method of filling mortar for villa with anti-cracking performance |
abstract | The invention relates to a method for preparing a filling mortar for villas with anti-cracking properties, comprising the following steps: mixing Portland cement, quartz sand, graphene hybrid modified nanowires, rare earth hybrid flake talc, phosphoric acid Aluminum dihydrogen and water were added to the mixer for stirring and mixing in turn to obtain the mortar base material; the mortar base material was kept at 45-55°C for 1-2h, and then placed in a plasma box for irradiation treatment, and the irradiation power was 100 -500W, the irradiation time is 25-35min, the irradiation is over, and the filling mortar for villas is obtained. The rare earth hybrid flaky talc powder added in the present invention is modified to the flaky talc powder, the activity is enhanced, and the raw materials are interspersed. In the process, the connection effect of the product is further improved, thereby improving the anti-cracking performance of the product, and the ratio of the raw materials in the present invention improves the strength and other properties of the product. |