http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114243102-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_44bcc470af955d2975eca32189830875 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2300-0091 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P70-50 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0565 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A62C3-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-058 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-46 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-058 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0565 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A62C3-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G77-46 |
filingDate | 2021-12-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9bdce8dbcba099471adc65318748c97f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_523f690a43dcd465819c80a515afbfc7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_77298f3a5dfe3dd354c4c934c09a7773 |
publicationDate | 2022-03-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-114243102-A |
titleOfInvention | Polysiloxane solid electrolyte, solid battery, preparation method and application thereof |
abstract | The invention provides a polysiloxane solid electrolyte, a solid battery, a preparation method and application thereof, wherein the preparation raw materials of the polysiloxane solid electrolyte comprise grafted polysiloxane, a polymer matrix, an inorganic filler and a lithium salt; the grafted polysiloxane obtained by copolymerizing the polymethylhydrosiloxane, the 1, 2-epoxy-4-vinylcyclohexane and the prenol polyoxyethylene ether effectively solves the problems of low ionic conductivity and poor mechanical property of the polysiloxane at room temperature, and the polymer matrix, the inorganic filler and the lithium salt are further matched, so that the obtained polysiloxane solid electrolyte not only has high flame retardant property, but also has excellent electrical property and thermal stability, can be applied to a lithium ion battery, and is beneficial to improving the electrical property of the lithium ion battery. |